Services · Custom Formulation
Custom Adhesive Formulation Tuned to Your Substrate, Climate and Cycle Time
When a standard grade doesn't fit your skin, your oven or your workshop climate, we change the formula, not your line. RELANET adjusts open time, activation temperature, solids, tack and heat limit for automotive interior parts, and supplies under your brand if you need it. Every custom automotive adhesive formulation starts from your substrate, your process and your OEM standard.

7 days
Custom samples for difficult substrates, in working days
1–2 months
Laboratory development to your standard, after we receive your substrates
NDA
Signed before you share materials or process data
Free
Custom samples; you buy production volumes
What We Can Adjust
A tailor-made adhesive for your production line starts from these parameters.
| Parameter | Why you'd change it | Example range today |
|---|---|---|
| Open time | Time for operators to position skins, or a short open time for fast robotic lines | R-5670: 8–15 min (hand) / 5–10 min (automated) · R-9610: 45–90 s |
| Activation temperature | Protect heat-sensitive skins, or tolerate oven drift on automated lines | R-5670: 65–85°C (hand) / 110–140°C window (automated) · R-5610: above 60°C |
| Solids | Coat weight, drying time and spray behavior | R-5670: 47–50% · R-5110 / R-5610: about 50% |
| Initial vs. final tack | Hold skins on curves straight from the press, or allow repositioning | R-5670: ~25 N/25 mm at 1 min, ~60 N/25 mm at 7 days |
| Color | Blue curing agent to see coverage while spraying; colorless for light or visible parts | R-60C blue or colorless |
| Heat limit | Sun-exposed parts vs. areas without direct sunlight | R-7110: 90°C design · R-7206: stable at 110°C |
| Packaging | Pack size matched to your consumption and handling | See packaging |
Open time
- Why you'd change it
- Time for operators to position skins, or a short open time for fast robotic lines
- Example range today
- R-5670: 8–15 min (hand) / 5–10 min (automated) · R-9610: 45–90 s
Activation temperature
- Why you'd change it
- Protect heat-sensitive skins, or tolerate oven drift on automated lines
- Example range today
- R-5670: 65–85°C (hand) / 110–140°C window (automated) · R-5610: above 60°C
Solids
- Why you'd change it
- Coat weight, drying time and spray behavior
- Example range today
- R-5670: 47–50% · R-5110 / R-5610: about 50%
Initial vs. final tack
- Why you'd change it
- Hold skins on curves straight from the press, or allow repositioning
- Example range today
- R-5670: ~25 N/25 mm at 1 min, ~60 N/25 mm at 7 days
Color
- Why you'd change it
- Blue curing agent to see coverage while spraying; colorless for light or visible parts
- Example range today
- R-60C blue or colorless
Heat limit
- Why you'd change it
- Sun-exposed parts vs. areas without direct sunlight
- Example range today
- R-7110: 90°C design · R-7206: stable at 110°C
Packaging
- Why you'd change it
- Pack size matched to your consumption and handling
- Example range today
- See packaging
Open time
Activation temperature
Solids
Initial vs. final tack
Color
Heat limit
When a Custom Formula Makes Sense
An adhesive for hard-to-bond substrates, a new process or a new skin usually means a custom formula.
| Situation | What usually needs to change |
|---|---|
| Hard-to-bond substrates: low-surface-energy PP, hard TPO, ultra-thin microfiber | Wetting and adhesion on the substrate; custom samples in 7 working days |
| Cycle time changes | Open time, activation time and green strength |
| Winter or humid workshops | Solids, activation temperature, open time |
| New processes: pre-coating, IR activation, robotic dispensing | Activation behavior and set speed |
| New skins: ultra-thin, ultra-soft, special-touch or light-transmitting skins | Activation temperature, elongation, optical properties |
| Light-colored or visible parts | Colorless curing agent, bleed-through control |
Hard-to-bond substrates: low-surface-energy PP, hard TPO, ultra-thin microfiber
- What usually needs to change
- Wetting and adhesion on the substrate; custom samples in 7 working days
Cycle time changes
- What usually needs to change
- Open time, activation time and green strength
Winter or humid workshops
- What usually needs to change
- Solids, activation temperature, open time
New processes: pre-coating, IR activation, robotic dispensing
- What usually needs to change
- Activation behavior and set speed
New skins: ultra-thin, ultra-soft, special-touch or light-transmitting skins
- What usually needs to change
- Activation temperature, elongation, optical properties
Light-colored or visible parts
- What usually needs to change
- Colorless curing agent, bleed-through control

Formulas We've Already Tuned
| What was tuned | Result | Where |
|---|---|---|
| Two versions of one 2K waterborne PU | Hand-wrapping version (8–15 min open time, 65–85°C activation, 600–1,000% elongation at 10°C) and automated version (5–10 min, 110–140°C window) | R-5670 |
| A PUR that activates at lower temperature | For heat-sensitive thin-wall plastics and soft foams | R-9692 |
| A high-initial-tack solution for a stressed part | Demold force held at the 45 N level; stopped stress debonding on curves and edge returns | Honda Ye S7 driver-side wrapped part |
| Curing-agent color | Blue for visual coat-weight control; colorless for appearance-critical parts | R-60C |
| Climate tuning | Solids, activation temperature and open time adjusted on site for South China's humid season and northern winters | Customer lines in China |
| A film designed for illuminated trim | >99% transmittance, ΔE ≈ 1.0 after 110°C × 1,500 h | RY-10, Honda Ye P7 / Ye S7 |
Two versions of one 2K waterborne PU
- Result
- Hand-wrapping version (8–15 min open time, 65–85°C activation, 600–1,000% elongation at 10°C) and automated version (5–10 min, 110–140°C window)
- Where
- R-5670
A PUR that activates at lower temperature
- Result
- For heat-sensitive thin-wall plastics and soft foams
- Where
- R-9692
A high-initial-tack solution for a stressed part
- Result
- Demold force held at the 45 N level; stopped stress debonding on curves and edge returns
- Where
- Honda Ye S7 driver-side wrapped part
Curing-agent color
- Result
- Blue for visual coat-weight control; colorless for appearance-critical parts
- Where
- R-60C
Climate tuning
- Result
- Solids, activation temperature and open time adjusted on site for South China's humid season and northern winters
- Where
- Customer lines in China
A film designed for illuminated trim
- Result
- >99% transmittance, ΔE ≈ 1.0 after 110°C × 1,500 h
- Where
- RY-10, Honda Ye P7 / Ye S7
Formulated for Your Climate
The same adhesive behaves differently in a humid summer in Guangzhou and a winter morning in the north. We adjust the formula for the plant, not just the product.
| Climate | What happens | What we adjust |
|---|---|---|
| Hot and humid (South China; similar conditions in Brazil and Southeast Asia) | Slow drying, white film after lamination, hydrolysis risk | Solids, activation temperature, open time; hydrolysis-resistant chemistry (R-5670: 85% retention after 60°C / 95% RH × 1,000 h) |
| Cold (northern China; Russia and Central Asia) | Longer activation, brittle film, frozen waterborne adhesive | Hot melt (APAO / PUR) recommended where frost can't be ruled out; waterborne adhesive only with storage and transport above 5°C; low-temperature elongation (600–1,000% at 10°C) |
Hot and humid (South China; similar conditions in Brazil and Southeast Asia)
- What happens
- Slow drying, white film after lamination, hydrolysis risk
- What we adjust
- Solids, activation temperature, open time; hydrolysis-resistant chemistry (R-5670: 85% retention after 60°C / 95% RH × 1,000 h)
Cold (northern China; Russia and Central Asia)
- What happens
- Longer activation, brittle film, frozen waterborne adhesive
- What we adjust
- Hot melt (APAO / PUR) recommended where frost can't be ruled out; waterborne adhesive only with storage and transport above 5°C; low-temperature elongation (600–1,000% at 10°C)

What We Need to Start
| Information | Why |
|---|---|
| Current adhesive or target grade | Starting point for the formula |
| Substrate and skin (materials and suppliers) | The material pair decides the bond |
| Part and location in the car | Heat, sunlight and stress |
| Application equipment and process | Spray, roll, dispense, film; oven and IR settings |
| Target cycle time | Open time and set speed |
| Durability and emission standard | The OEM tests the formula must pass |
| Volume estimate: annual vehicles × adhesive per vehicle | Lets us size the project and plan supply |
| Signed NDA | Before you share materials, drawings or process data |
| 1–2 m² of skin and substrate | For laboratory development and flat-panel tests |
Current adhesive or target grade
- Why
- Starting point for the formula
Substrate and skin (materials and suppliers)
- Why
- The material pair decides the bond
Part and location in the car
- Why
- Heat, sunlight and stress
Application equipment and process
- Why
- Spray, roll, dispense, film; oven and IR settings
Target cycle time
- Why
- Open time and set speed
Durability and emission standard
- Why
- The OEM tests the formula must pass
Volume estimate: annual vehicles × adhesive per vehicle
- Why
- Lets us size the project and plan supply
Signed NDA
- Why
- Before you share materials, drawings or process data
1–2 m² of skin and substrate
- Why
- For laboratory development and flat-panel tests
How a Custom Project Runs
- 1
Step 1: Information review
- What happens
- We review your materials, process and standard
- Time
- —
- 2
Step 2: NDA
- What happens
- Signed by both sides
- Time
- —
- 3
Step 3: Materials received
- What happens
- Your skin and substrate in our lab
- Time
- —
- 4
Step 4: Laboratory development
- What happens
- Formula adjusted and tested to your standard documents
- Time
- 1–2 months (custom samples for difficult substrates in 7 working days)
- 5
Step 5: Flat-panel report
- What happens
- Peel, aging and other results against your target
- Time
- —
- 6
Step 6: Trial on your line
- What happens
- Engineers on site; then the eight-step route to SOP
No fixed MOQ: production volumes are agreed per project.
OEM and Private Label Supply
RELANET Formulations Under Your Brand
Building your own adhesive line for automotive interiors? We produce RELANET-qualified formulations under your brand.
| What you get | Detail |
|---|---|
| Your brand | Your label and your product name |
| Your documents | TDS, SDS and COA prepared in your format |
| Confidentiality | Formulation and your process know-how kept confidential under NDA |
| Same quality control | Batch testing, retained samples (about 250 ml per batch) and change control as for our own grades |
| Quality system | IATF 16949 (IATF/T19001-2026), ISO 9001, ISO 14001, ISO 45001 |
| Capacity | About 960 t per year |
Your brand
- Detail
- Your label and your product name
Your documents
- Detail
- TDS, SDS and COA prepared in your format
Confidentiality
- Detail
- Formulation and your process know-how kept confidential under NDA
Same quality control
- Detail
- Batch testing, retained samples (about 250 ml per batch) and change control as for our own grades
Quality system
- Detail
- IATF 16949 (IATF/T19001-2026), ISO 9001, ISO 14001, ISO 45001
Capacity
- Detail
- About 960 t per year
Packaging Built Around Your Line
Pack sizes can be customized to your consumption and handling.
| Product | Standard format | Notes |
|---|---|---|
| PUR hot melt | 20 kg pails | Sealed against moisture; 9-month shelf life at 5–35°C |
| Adhesive film (RY-10) | Rolls from 1 roll (100 m²) | 40–200 µm thickness; die-cut shapes on request |
| Waterborne adhesives | See TDS | Shipped with frost protection, kept above 5°C |
| Custom | Sized to your line | Discuss with us |
PUR hot melt
- Standard format
- 20 kg pails
- Notes
- Sealed against moisture; 9-month shelf life at 5–35°C
Adhesive film (RY-10)
- Standard format
- Rolls from 1 roll (100 m²)
- Notes
- 40–200 µm thickness; die-cut shapes on request
Waterborne adhesives
- Standard format
- See TDS
- Notes
- Shipped with frost protection, kept above 5°C
Custom
- Standard format
- Sized to your line
- Notes
- Discuss with us
Your Process Stays Yours
NDA before data. We sign before you send materials, drawings or process parameters.
Your process isn't shared. Customer process details, photos and videos from your line are never published.
Our formulas aren't disclosed either. Formulations, raw materials and equipment brands stay confidential, which protects the consistency of what we supply you.
Changes are controlled. Once a custom formula is approved, changes follow written change control with advance notice.
Frequently Asked Questions
Custom formulas, including adhesive for hard-to-bond substrates: what we change, how long it takes and how supply works.
What can you change in a custom formula?
Open time, activation temperature, solids, the balance of initial and final tack, curing-agent color, heat limit and packaging.
How long does custom development take?
Custom samples for difficult substrates in 7 working days; laboratory development to your standard in 1–2 months after we receive your materials.
Do you sign an NDA?
Yes, before you share materials or process data.
Is there a minimum order for custom formulas?
No fixed MOQ. Production volumes are agreed per project, based on your annual vehicle volume and adhesive per vehicle.
Do custom samples cost anything?
No. Custom samples are free; production volumes are purchased.
Can you supply under our brand?
Yes. We produce RELANET-qualified formulations under your label and product name, with documents in your format.
Can packaging be customized?
Yes. Pack sizes are matched to your consumption and handling.
Start a Custom Project
Send us your substrate, skin, process, cycle time and OEM standard. We'll sign an NDA, review the project and tell you what can be tuned.
An engineer replies within 1 working day.