Applications › Door & Instrument Panels
Wrapping Adhesives for Door Panels, Instrument Panels, Armrests and Pillars
Soft-touch skins on door panels and dashboards are where buyers judge an interior, and where bonding is hardest: deep draws, folded edges, tight radii and years of sun. RELANET's door panel wrapping adhesive, R-5670, reaches about 25 N/25 mm peel one minute after lamination and runs in series production on Nissan N7 programs and GAC Toyota Camry door panels.
- Peel at 1 minute (R-5670)
- ~25 N/25 mm
- Microfiber on ABS, 180° peel
- ≥1,150 N/m
- After −40°C × 24 h
- 92% retention

The Problem
"The skin looked perfect off the press. Three months later, the edges lifted."
Wrapped panels fail in predictable places:
Folded edges spring back. The skin pulls away at hems and turned edges, especially on PVC with a stiff knit backing.
Blisters after demolding or after sun. Hot demolding, uneven mold gaps or weak green strength leave bubbles that grow with heat.
Deep draws tear or wrinkle. On instrument panels the skin stretches hard, and a brittle adhesive film cracks with it.
Winter cracking. In cold workshops and cold climates, low elongation means skins crack at radii.
Odor failures. The panel passes peel tests, then fails the OEM's odor or VOC test.
The adhesive gets blamed. Most failures start at the interface: expired surface treatment, release agent, a different skin lot. Without testing, nobody knows.
Door panel wrapping adhesive
Door Panels and Inserts
A door panel wrapping adhesive has to hold folded hems, inserts and trim strips through daily contact and sun.
- Conditions: folded hems, inserts and trim strips, frequent contact with hands and cleaning products, sun through the side window.
- Common failures: edge lifting at hems, blistering on the upper panel, skins shifting during wrapping.
| Recommended | Why |
|---|---|
| R-5670 2K waterborne PU | Fast green strength holds folded edges; low VOC; proven on Nissan N7 / N6 / NX7 and GAC Toyota Camry door panels |
| R-7110 APAO hot melt | Door inserts, trim strips and fabric edge folding; bonds PP and ABS without primer; proven on Dongfeng Nissan Sylphy |
- Key data: folded edges show no debonding after 1,000 bends; PVC on wood-plastic board ≥1,050 N/m; 72 h in interior cleaner causes <6% strength loss.
- Process tip: for hand-wrapped door panels, wrap from the lowest point of the deepest cavity outward to the edge, keep tongue-and-groove features to a minimum so they don't block the hem, and allow at least 5 mm of skin for the turned edge.

Instrument panel skin adhesive · Dashboard wrapping adhesive
Instrument Panels and Dashboards
An instrument panel skin adhesive, or dashboard wrapping adhesive, does the most demanding job in the cabin: large, deep, curved shapes on the hottest surface, under the windshield.
- Conditions: the hottest surface in the cabin, under the windshield; large, deep, curved shapes; the most adhesive per vehicle and the most demanding part technically.
- Common failures: voids and bubbles deep in 3D curves after vacuum forming, edge lifting after heat aging, skin wrinkles.
| Recommended | Why |
|---|---|
| R-5670 2K waterborne PU (automated version) | Wide activation window (110–140°C) keeps green strength stable when oven temperature drifts; holds at −0.09 to −0.1 MPa vacuum |
| R-9610 reactive PUR | ≥500% elongation follows the skin on deep draws; 91.3% retention after 85°C / 95% RH × 1,000 h; low odor (VDA 270 2.5–3.0) |
R-5670 2K waterborne PU (automated version)
- Why
- Wide activation window (110–140°C) keeps green strength stable when oven temperature drifts; holds at −0.09 to −0.1 MPa vacuum
R-9610 reactive PUR
- Why
- ≥500% elongation follows the skin on deep draws; 91.3% retention after 85°C / 95% RH × 1,000 h; low odor (VDA 270 2.5–3.0)
- Key data: TPO on modified PP ≥980 N/m; 105°C × 24 h retention 88%; vacuum dwell 40–90 s for automatic de-bubbling of 3D curves.
- Process tip: instrument panels are usually vacuum formed or hot pressed. Control mold gaps against adhesive thickness, give the infrared a second activation, and cool before demolding; hot demolding is a common cause of blisters.

Armrest wrapping adhesive
Center Consoles and Armrests
An armrest wrapping adhesive has to follow tight radii and hold leather and microfiber skins under daily pressure and rubbing.
- Conditions: tight radii and bends, leather and microfiber skins, pressure and rubbing every day.
- Common failures: lifting at bends, oily shine after sun, stitched skins shifting.
- Key data: microfiber on ABS ≥1,150 N/m; no color change, oil bleed or migration after 85°C × 500 h.

Pillar Trim
- Conditions: narrow, curved parts wrapped all round; exposure to cold in northern climates.
- Common failures: cracking and lifting in severe cold, lifting on narrow returns.

Matching the Adhesive to Your Process
| Process | Best for | Watch out for | Recommended |
|---|---|---|---|
| Hand wrapping | Small and medium parts with complex shapes; keep parts within about 80 × 40 cm | Consistency between operators; flame-treated PP must be wrapped within 4 hours | R-5670 hand-wrapping version |
| Hot press | High consistency; shared lines | Mold gap, IR activation and cooling | R-5670 (high initial tack) |
| Silicone membrane vacuum press | Stitched parts; low tooling cost | No way to measure or cool the bond line, so initial tack does the holding | R-5670 |
| IMG (in-mold graining) | Visible, high-grain parts | Tooling and TPO skin cost | R-5670 |
| Vacuum forming (automated) | Large instrument panels | Voids in deep 3D areas | R-5670 automated version, R-9610 |
| Hot melt roll coating | Solvent-free, waste-free lines | Equipment cleaning; wrinkles on stretched skins | R-7110, R-9610 |
Hand wrapping
- Best for
- Small and medium parts with complex shapes; keep parts within about 80 × 40 cm
- Watch out for
- Consistency between operators; flame-treated PP must be wrapped within 4 hours
- Recommended
- R-5670 hand-wrapping version
Hot press
- Best for
- High consistency; shared lines
- Watch out for
- Mold gap, IR activation and cooling
- Recommended
- R-5670 (high initial tack)
Silicone membrane vacuum press
- Best for
- Stitched parts; low tooling cost
- Watch out for
- No way to measure or cool the bond line, so initial tack does the holding
- Recommended
- R-5670
IMG (in-mold graining)
- Best for
- Visible, high-grain parts
- Watch out for
- Tooling and TPO skin cost
- Recommended
- R-5670
Vacuum forming (automated)
- Best for
- Large instrument panels
- Watch out for
- Voids in deep 3D areas
- Recommended
- R-5670 automated version, R-9610
Hot melt roll coating
- Best for
- Solvent-free, waste-free lines
- Watch out for
- Equipment cleaning; wrinkles on stretched skins
- Recommended
- R-7110, R-9610
The Stack Behind a Wrapped Panel
- 1Skin (PVC with knitted backing)
- 2Adhesive layer (R-5670)
- 3Flame-treated PP substrate
Define the Skin, Not Just the Adhesive
With the same adhesive and the same process, two PVC skins with knitted backing gave very different results: 12.7 N on one and 7.6 N on the other, a 66.8% difference. The adhesive bonds to the knit fabric on the back of the PVC, so the knit's material and structure decide much of the peel strength.
That is why we test your exact skin and substrate first, and why we recommend locking the skin specification before adhesive approval.
- PVC skin A12.7 N
- PVC skin B7.6 N
Durability Data
| Test | Result | Condition |
|---|---|---|
| Multi-substrate 180° peel | ≥1,150 N/m microfiber / ABS; ≥980 N/m TPO / modified PP; ≥1,050 N/m PVC / wood-plastic board | 24 h after cure |
| Humidity aging | 85% peel retention | 60°C / 95% RH × 1,000 h |
| Low temperature | 92% retention | −40°C × 24 h |
| High temperature | 88% retention | 105°C × 24 h |
| Thermal cycling | No delamination; 85% retention | 100 cycles, −40°C ↔ 105°C |
| Heat and sun | No color change, oil bleed or migration | 85°C × 500 h |
| Chemical resistance | <6% strength loss | 72 h in neutral interior cleaner and silicone care fluid |
| Folded-edge bending | No debonding after 1,000 bends | Door panel hem |
Multi-substrate 180° peel
- Result
- ≥1,150 N/m microfiber / ABS; ≥980 N/m TPO / modified PP; ≥1,050 N/m PVC / wood-plastic board
- Condition
- 24 h after cure
Humidity aging
- Result
- 85% peel retention
- Condition
- 60°C / 95% RH × 1,000 h
Low temperature
- Result
- 92% retention
- Condition
- −40°C × 24 h
High temperature
- Result
- 88% retention
- Condition
- 105°C × 24 h
Thermal cycling
- Result
- No delamination; 85% retention
- Condition
- 100 cycles, −40°C ↔ 105°C
Heat and sun
- Result
- No color change, oil bleed or migration
- Condition
- 85°C × 500 h
Chemical resistance
- Result
- <6% strength loss
- Condition
- 72 h in neutral interior cleaner and silicone care fluid
Folded-edge bending
- Result
- No debonding after 1,000 bends
- Condition
- Door panel hem
Typical lab values for RELANET waterborne PU; test conditions stated. Validate on your substrate, process and OEM standard.
Proven in Series Production
A problem we solved: on the Nissan NX7 program, the door panel line moved from solvent adhesive to waterborne. Early peel was only 5–10 N against a 19 N target. Cross-testing traced the cause to the skin's knit fabric, not the adhesive. Adding a nonwoven layer met the target.
Frequently Asked Questions
Which adhesive should I use for door panel wrapping?
R-5670 2K waterborne PU for most hand-wrapped, hot-pressed and vacuum-formed door panels. Use R-7110 APAO hot melt for inserts, trim strips and fabric edge folding on PP or ABS.
Why do my folded edges lift?
Usually it is weak green strength, too little skin left for the hem (keep at least 5 mm), or expired surface treatment on PP. We test each cause on your part.
What's best for deep-draw instrument panels?
The automated R-5670 version, with its wide activation window, or R-9610 PUR when you need very high elongation.
Can operators reposition the skin during hand wrapping?
Yes. The hand-wrapping version of R-5670 has an 8–15 minute open time.
Do I need to treat PP before wrapping?
With waterborne PU, yes: flame, corona or plasma treatment, then wrap within 4 hours. R-7110 hot melt can bond qualified clean PP without pretreatment.
Will it pass my OEM's odor test?
R-5670 measured 2 g/L VOC (SGS) and odor intensity 2.3 by the Nissan VES method. We run pre-validation testing to your OEM's standard before you submit.
Send Us Your Skin and Substrate
Send 1–2 m² of your skin and substrate. We'll run a free flat-panel peel test, recommend a grade and process window, then support your first trial on real parts.