RELANETRELANET

Lamination Processes

Matching the Interior Wrapping Adhesive to Your Lamination Process

There is no best process, only the process that fits your part, your materials and your volume. The process and the adhesive have to be chosen together. We qualify interior wrapping adhesives for six lamination routes plus robotic application, and we start where most failures start: the substrate interface.

Hot press mold opening with a freshly wrapped automotive door panel

Six Processes at a Glance

  • Hand wrapping

    Consistency
    Low
    Up-front investment
    Low
    Main advantage
    Flexible, low cost
    Main risk / cost
    Operator-to-operator variation; part size limit about 80 × 40 cm
    Recommended
    R-5670 hand-wrapping version
  • Hot press

    Consistency
    High
    Up-front investment
    High
    Main advantage
    High consistency, shared lines
    Main risk / cost
    Expensive molds; poor temperature control causes batch debonding
    Recommended
    R-5670 (high initial tack)
  • Silicone membrane vacuum press

    Consistency
    Medium
    Up-front investment
    Low
    Main advantage
    Friendly to stitched parts, low cost
    Main risk / cost
    Grain damage, membrane fatigue, no cooling
    Recommended
    R-5670
  • IMG vacuum forming

    Consistency
    High
    Up-front investment
    High
    Main advantage
    Sharpest, most even grain
    Main risk / cost
    Expensive molds and TPO skins
    Recommended
    R-5670
  • Hot melt roll coating

    Consistency
    High
    Up-front investment
    High
    Main advantage
    No solvent, no hazardous waste, shared lines
    Main risk / cost
    Equipment cleaning; wrinkles on stretched skins
    Recommended
    R-7110, R-7206, R-9610
  • Pre-coated adhesive film

    Consistency
    Highest
    Up-front investment
    High
    Main advantage
    Zero emissions, predictable, long storage, lower cost
    Main risk / cost
    Needs four parties to align
    Recommended
    RY-10

Want this chart as a one-page PDF for your team?

Before Any Process: Surface Pretreatment

90% of Debonding Starts at the Interface, Not in the Adhesive

All six routes start with the substrate. Four things cause most failures:

  1. 1.PP and IXPP wet poorly. Their surface energy is only about 24 mN/m. They need flame, corona or plasma treatment, and the treatment doesn't last.

  2. 2.Mold-release residue. The adhesive bonds to the release agent instead of the part, and the whole skin peels after aging.

  3. 3.Changing regrind ratios. More or less recycled material changes the surface, and consistency is lost.

  4. 4.Workshop contamination. Dust, oil and fingerprints start interface failure.

  • PP / IXPP

    Surface energy
    ~24 mN/m (hard to bond)
  • ABS / PC+ABS

    Surface energy
    ~28–32 mN/m
  • RELANET PU adhesive layer

    Surface energy
    ~32 mN/m
  • Target for the substrate

    Surface energy
    ≥38 mN/m (cohesive failure)
Surface energy scale (mN/m)
  • PP / IXPP~24 mN/m (hard to bond)
  • ABS / PC+ABS~28–32 mN/m
  • RELANET PU adhesive layer~32 mN/m
  • Target for the substrate≥38 mN/m (cohesive failure)

The key point: a good dyne reading doesn't mean a good bond. After flame or plasma treatment, wrap within 4 hours. The active surface groups fade over time while the dyne reading stays the same, which is very easy to misjudge. High workshop temperatures speed up the loss. Put the treatment time window into your control plan, not only the dyne level.

Surface pretreatment steps

  1. 1Keep the surface free of mold-release residue, dust, oil and fingerprints.
  2. 2Treat PP and IXPP with flame, corona or plasma: their surface energy is only about 24 mN/m.
  3. 3Bring the substrate to the target surface energy of ≥38 mN/m.
  4. 4Wrap within 4 hours of flame or plasma treatment. High workshop temperatures speed up the loss of activity.
  5. 5Put the treatment time window into your control plan, not only the dyne level.
Flame treatment of a PP substrate and a dyne pen surface-energy check before wrapping
4-hour window

No pretreatment option: R-7110 and R-7206 APAO hot melts bond PP and ABS directly, without sanding or primer. PP primers R-132 and R-136 are available when pretreatment is required.

Hand Wrapping

Hand wrapping is where most teams choose their first hand wrapping adhesive for automotive interior parts, and where switching from solvent to waterborne PU changes the process.

Typical process with waterborne PU:

  1. 1PP substrate pretreatment (flame or plasma) (Added step)
  2. 2Spray substrate
  3. 3Spray skin
  4. 4Oven drying (Added step)
  5. 5Hand wrapping

Added step

Compared with the solvent process (spray substrate → spray skin → flash off solvent → wrap), switching to waterborne adds two steps: pretreatment and oven drying.

Four points teams most often miss when switching to waterborne:

  • A good dyne reading doesn't mean a good bond. Wrap within 4 hours of treatment, and remember high temperatures also strip the active groups.
  • Wrap from the lowest point of the deepest cavity outward to the edge, to avoid bubbles and stress.
  • Keep tongue-and-groove features to a minimum so they don't block the hem.
  • Treat it as a hand-wrapped part and keep it small: about 80 × 40 cm or less.
Pros
Flexible, low cost
Cons
Poor consistency; on large parts the front and back heat up differently, so the adhesive activates unevenly
Recommended
R-5670 hand-wrapping version: open time 8–15 min, activation 65–85°C, 600–1,000% elongation at 10°CR-5670

Hot Press

A hot press lamination adhesive needs high initial tack: too little causes batch debonding, so we recommend the R-5670 high-initial-tack version for hot press lines.

Process:

  1. 1Substrate pretreatment
  2. 2Spray substrate
  3. 3Spray skin
  4. 4Oven drying
  5. 5Place materials in the mold
  6. 6Second infrared activation
  7. 7Close the mold
  8. 8Hold pressure
  9. 9Cool
  10. 10Demold

Six difficulties:

  • Uneven mold gaps, so pressing force varies across the part.
  • Heating that damages the skin; deep shapes or skins with too little stretch.
  • No mold cooling, so parts demold too hot and blister or debond.
  • Too little initial tack, causing batch debonding.
  • Less than 5 mm left for the turned edge.
  • Poor understanding of how PVC single-grain skins and woven fabrics behave.
Hot press lamination mold for an automotive interior trim part

Case: Honda Ye S7 driver-side wrapped part. The part combines continuous curves with edge returns, so stress concentrates at the curve inflection points and the returned edges. It is a hard test of initial tack and stretch. Stress debonding in production was solved with a high-initial-tack formulation that holds demolding force steady at around 45 N.

~45 N

Demolding force

Pros
High consistency, can share lines
Cons
Expensive molds that are hard to repair
Recommended
R-5670 high-initial-tack versionR-5670
Hot press money goes into the mold. Points are lost on temperature control: gap, activation, cooling — skip none of them.

Silicone Membrane Vacuum Press

Process:

  1. 1Substrate pretreatment
  2. 2Spray substrate
  3. 3Spray skin
  4. 4Oven drying
  5. 5Pre-position the skin
  6. 6Place on the mold
  7. 7Silicone membrane vacuum (8 bar)
  8. 8Infrared heating of the whole part
  9. 9Demold

Hidden risks:

  • The adhesive is activated by heat passing through the skin, so you can't directly confirm it reached temperature.
  • Grain damage on the skin; too much pressure distorts the substrate.
  • No way to cool and set the adhesive, so initial tack has to do the holding.
  • Membrane fatigue can't be predicted, and replacement timing is a matter of experience.
  • Height differences in the part load the membrane unevenly and can even tear it.
Pros
Good for stitched parts, low cost
Cons
Can damage skin appearance; needs regular maintenance
Recommended
R-5670, where high initial tack compensates for the lack of coolingR-5670

IMG (In-Mold Graining) Vacuum Forming

IMG is the vacuum forming route for automotive interior parts where grain quality matters most, and R-5670 is our recommended vacuum forming adhesive for automotive IMG parts.

Process:

  1. 1Substrate pretreatment
  2. 2Spray substrate
  3. 3Spray skin
  4. 4Ceramic-plate heating
  5. 5Grain forming on the skin
  6. 6Close the mold
  7. 7Hold pressure
  8. 8Demold

Ceramic-plate heating with negative vacuum forming creates the grain directly on the skin side. Grain sharpness and evenness are the best of all the vacuum and press routes, which suits high-visibility driver-side parts. Unlike the membrane route, the skin grain is not pressed a second time.

Pros
Sharp, even grain
Cons
Expensive molds and TPO skins
Recommended
R-5670R-5670

Hot Melt Roll Coating

Process:

  1. 1Substrate pretreatment
  2. 2Roll-coat adhesive onto the skin (APAO or PUR)
  3. 3Second infrared activation
  4. 4Press
  5. 5Cool
  6. 6Demold

Difficulties:

  • Equipment cleaning is a burden: hot melt lines and rollers need regular cleaning.
  • High up-front investment in roll coaters and temperature control.
  • Skins wrinkle when stretched; deep parts are limited.
  • Usually only two adhesive types: APAO (long open time, good heat resistance) or PUR (high initial tack plus moisture crosslinking).
Pros
No solvent, no hazardous waste, can share lines
Cons
High investment, demanding maintenance
Recommended
R-7110 (long open time, PP without primer), R-7206 (110°C), R-9610 PURR-7110, R-7206, R-9610

Case: Honda Ye S7 driver-side wrapped part. With continuous curves and returned edges, stress concentrates at the inflection points and edge returns. Production stress debonding on this part was solved by a high-initial-tack solution outside the roll-coating system, holding demolding force at around 45 N. Sometimes the right answer is a different adhesive, not a different setting.

Platform Pre-Coated Adhesive Film

The Future Process: Turn the Bond Line Into a Supplied Material

Process:

  1. 1Pre-coat the skin roll (with release liner)
  2. 2Computer nesting and cutting
  3. 3Substrate pretreatment
  4. 4Load the mold
  5. 5Infrared activation
  6. 6Press
  7. 7Hold
  8. 8Cool
  9. 9Demold

The core difficulty is coordination. The skin supplier, adhesive supplier, Tier 1 and OEM must agree on pre-coating parameters, release liners, cutting layouts, activation windows and storage time. If any one of them drops out, the platform can't launch. The up-front investment is high, but once it runs, process cost falls significantly.

Pros
Highest consistency, zero emissions, predictable, long storage
Cons
High up-front investment; hardest to organize
Recommended
RY-10 film: thickness, area and edges are set at the supplier, so the line only peels, positions and pressesRY-10
Cost example:
  • Pre-coated filmRMB 12.5/m²
  • SprayingRMB 14.8/m²

Cost example: film came to RMB 12.5/m² against RMB 14.8/m² for spraying, once labor, exhaust treatment and waste were counted (industry illustration).

Robotic Spraying and Dispensing

Hand-wrapping know-how doesn't transfer to robots. Automated lines need an adhesive with a predictable activation window and fast strength build-up.

Robotic spraying (waterborne PU):

Process:

  1. 1Robotic spraying
  2. 2Drying and activation
  3. 3Second infrared activation
  4. 4Mesh-fabric lamination
  5. 5Pressing and forming

We record dimensions, coat weight, temperature and cycle time, and turn validated settings into work instructions. On automated lines, R-5670's activation window of 110–140°C keeps green strength stable when oven temperature drifts.

Robotic hot melt dispensing:

R-7206 has precise temperature control and fast strength build-up for sunroof frames, brackets and stiffeners, with no pretreatment on ABS or PP.

Robot spraying R-5670 waterborne PU adhesive on an interior trim substrate
R-5670 robotic spraying with blue curing agent and vacuum forming

What We Recommend to OEMs

Define the Process, Materials, Standards and Controls

OEMs see the market and the vehicle program further ahead than anyone in the supply chain. Their definitions set the limits of what the supply chain can develop. We recommend that OEMs define four things directly:

  1. 1

    Process. Choose hand wrapping, hot press, membrane press, IMG, roll coating or pre-coating based on part shape and volume.

  2. 2

    Materials. Lock the substrate, skin specification and adhesive system, so the adhesive isn't blamed when the skin changes.

  3. 3

    Standards. Write peel strength, aging, VOC, surface energy and the treatment time window into the standard, as a common language for the whole supply chain.

  4. 4

    Control methods. DOE windows, SPC, incoming inspection and batch traceability, built into the process.

Why it matters, with data. With the same process and the same adhesive, two PVC skins with knitted backing gave average peels of 12.7 N and 7.6 N, a 66.8% difference. The adhesive bonds to the knit fabric on the back of the PVC, so the difference comes from the fabric, not the glue. If the materials aren't defined, the data can't be compared.

Average peel, same process and same adhesive (N)
  • PVC skin A (knitted backing)12.7 N
  • PVC skin B (knitted backing)7.6 N

66.8% difference

Keep current and potential suppliers qualified together. An OEM's ability to define is the supply chain's ability to develop.

How We Work on Your Process

  1. 01

    Flat-panel screening on 1–2 m² of your skin and substrate, testing materials and environment only.

  2. 02

    Trial on your real parts and equipment.

  3. 03

    Record process parameters: dimensions, coat weight, temperature, cycle time.

  4. 04

    Part-level test data you can submit to the OEM.

  5. 05

    Work instructions if the result is OK; if not, we revise and repeat.

  6. 06

    SOP with production follow-up.

We run a joint DOE with you to find the production window for temperature, pressure and time. The process window is the last mile where adhesive performance is won or lost.

Want our process parameter record template?

Frequently Asked Questions

  • Which interior wrapping adhesive suits my process?

    Waterborne PU (R-5670) for hand wrapping, hot press, membrane press, IMG and robotic spraying. APAO (R-7110, R-7206) or PUR (R-9610) for roll coating. RY-10 film for pre-coated lamination.

  • Why do parts blister after hot pressing?

    Common causes are uneven mold gaps, demolding while the part is still hot, weak initial tack, or treated PP left too long before wrapping.

  • How long can treated PP wait before wrapping?

    Wrap within 4 hours. The dyne reading may still look fine after the surface has lost its activity.

  • Is a membrane press worse than a hot press?

    Not worse, but different: it is cheaper and stitch-friendly, yet you can't cool the bond line, so initial tack matters more.

  • Can you help us move to an automated line?

    Yes. We tune activation settings and record parameters on your equipment, and turn them into work instructions.

Tell Us Your Process

Share your part, skin, substrate, equipment and cycle time. We'll recommend the adhesive and the process window, and support your first trial on the line.

anson@relanetadhesive.com