Products › 2K Waterborne PU
2K Waterborne Polyurethane (PUD) Adhesive for Interior Trim Wrapping
RELANET R-5670 with R-60C curing agent bonds PVC, PU leather, TPO, microfiber and fabric skins to PP, ABS and honeycomb substrates. It reaches about 25 N/25 mm peel one minute after lamination, measures 2 g/L VOC, and runs in series production on Nissan N7 programs and BYD Denza Z9GT.
- ~25 N/25 mm
- Peel at 1 minute
- 2 g/L VOC
- SGS, GB 33372 (limit 50 g/L)
- 85% retention
- After 60°C / 95% RH × 1,000 h
- 0
- Customer complaints on Nissan N7 since series production

“Our waterborne adhesive is either too slow on the press or too weak after aging.”
Interior wrapping lines that use waterborne PU run into the same issues again and again:
Slow green strength. Parts sit in the press, or the skin springs back at folded edges before the bond sets.
Odor and VOC failures. The bond passes peel tests, then fails the OEM’s odor test late in validation.
Humidity and heat aging. Bonds that look fine at the end of the line blister or lift after a humid summer or a hot parking lot.
Cold workshops. Skins tear on curved edges in winter because the adhesive film loses elongation.
No visual control of coat weight. Operators can’t see how much they have sprayed, so coat weight drifts from shift to shift.
R-5670: A Second-Generation 2K Waterborne PU Built Around Green Strength and Clean Emissions
A waterborne polyurethane adhesive for automotive interior wrapping, designed so the part leaves the press sooner and passes the OEM odor test.
Fast initial tack.
About 25 N/25 mm at 1 minute and about 60 N/25 mm at 7 days (PVC with knitted backing on flame-treated PP), so parts leave the press sooner.
Low VOC, low odor.
2 g/L VOC by SGS. By the Nissan VES method, odor intensity is 2.3 with zero irritation, and formaldehyde, acetaldehyde, benzene series and TVOC are not detected.
Durable after aging.
Passed BYD interior testing at 90°C × 168 h and 10 humidity-temperature cycles, with substrate failure in every test.
Blue curing agent you can see.
The blue R-60C shows coat weight at a glance. A clear curing agent is available for light-colored parts where no tint is allowed.
Tuned to your process.
Hand-wrapping and automated-line versions; open time, activation temperature, solids and tack balance adjustable. Custom samples in 7 working days.
RELANET R-5670 2K Waterborne PU Adhesive
Technical data for this water-based polyurethane adhesive (PUD) for automotive interior trim, used with R-60C curing agent.
| Item | Typical value |
|---|---|
| Chemistry | Second-generation two-component waterborne polyurethane dispersion |
| Curing agent | R-60C (blue); clear version available |
| Mixing ratio | R-5670 : R-60C = 100 : 5–8 by weight (see current TDS) |
| Solids | 47%–50% |
| Peel at 1 minute | ~25 N/25 mm (25 mm width, timed from end of lamination) |
| Peel at 7 days | ~60 N/25 mm |
| Test combination | PVC with knitted backing / flame-treated PP |
| Pot life after mixing | See current TDS |
| Application | Spray (manual or robotic), with oven drying and IR activation |
| Processes | Hand wrapping, hot press, silicone membrane vacuum press, vacuum forming |
| Substrates | PP (flame-treated), ABS, PC/ABS, PHC paper honeycomb (sand-blasted) |
| Skins | PVC, PU leather, TPO, microfiber, 3D mesh, flocked fabric, knitted fabric |
| VOC content | 2 g/L (GB 33372-2020, SGS GZAT2603001821PC01) |
| Odor | Intensity 2.3, irritation 0 (Nissan VES M00-08, 90°C × 4 h, SGS) |
| Packaging | Standard drums with matching curing-agent packs; pack sizes customized to your consumption |
| Storage | Above 5°C; waterborne adhesive is damaged irreversibly by freezing below 4°C |
Chemistry
- Typical value
- Second-generation two-component waterborne polyurethane dispersion
Curing agent
- Typical value
- R-60C (blue); clear version available
Mixing ratio
- Typical value
- R-5670 : R-60C = 100 : 5–8 by weight (see current TDS)
Solids
- Typical value
- 47%–50%
Peel at 1 minute
- Typical value
- ~25 N/25 mm (25 mm width, timed from end of lamination)
Peel at 7 days
- Typical value
- ~60 N/25 mm
Test combination
- Typical value
- PVC with knitted backing / flame-treated PP
Pot life after mixing
- Typical value
- See current TDS
Application
- Typical value
- Spray (manual or robotic), with oven drying and IR activation
Processes
- Typical value
- Hand wrapping, hot press, silicone membrane vacuum press, vacuum forming
Substrates
- Typical value
- PP (flame-treated), ABS, PC/ABS, PHC paper honeycomb (sand-blasted)
Skins
- Typical value
- PVC, PU leather, TPO, microfiber, 3D mesh, flocked fabric, knitted fabric
VOC content
- Typical value
- 2 g/L (GB 33372-2020, SGS GZAT2603001821PC01)
Odor
- Typical value
- Intensity 2.3, irritation 0 (Nissan VES M00-08, 90°C × 4 h, SGS)
Packaging
- Typical value
- Standard drums with matching curing-agent packs; pack sizes customized to your consumption
Storage
- Typical value
- Above 5°C; waterborne adhesive is damaged irreversibly by freezing below 4°C
Typical values on tested specimens. Validate on your substrate, process and OEM standard.
Matched to Hand Wrapping or Automated Lines
| Item | Hand-wrapping version | Automated-line version |
|---|---|---|
| Typical use | Complex curves, tight corners, folded edges, smaller parts | Vacuum forming and automated wrapping lines |
| Open time | 8–15 min | 5–10 min |
| Activation | 65–85°C | Wide window of 110–140°C; full green strength in 40–60 s at 120–130°C |
| Low-temperature elongation | 600–1,000% at 10°C | — |
| Vacuum | — | Holds at −0.09 to −0.1 MPa; 40–90 s vacuum dwell |
| Drying | Room-temperature crosslinking in 24 h | Staged drying 60°C → 80°C |
Typical use
- Hand-wrapping version
- Complex curves, tight corners, folded edges, smaller parts
- Automated-line version
- Vacuum forming and automated wrapping lines
Open time
- Hand-wrapping version
- 8–15 min
- Automated-line version
- 5–10 min
Activation
- Hand-wrapping version
- 65–85°C
- Automated-line version
- Wide window of 110–140°C; full green strength in 40–60 s at 120–130°C
Low-temperature elongation
- Hand-wrapping version
- 600–1,000% at 10°C
- Automated-line version
- —
Vacuum
- Hand-wrapping version
- —
- Automated-line version
- Holds at −0.09 to −0.1 MPa; 40–90 s vacuum dwell
Drying
- Hand-wrapping version
- Room-temperature crosslinking in 24 h
- Automated-line version
- Staged drying 60°C → 80°C
Typical lab values from RELANET technical publications; test conditions stated. Your version is set during sampling.
Why it matters: a longer open time gives operators time to reposition the skin on a curved armrest. A wide activation window keeps green strength stable when oven temperature drifts on an automated line.
How R-5670 Runs on a Door-Panel Line
A typical robotic door-panel wrapping sequence (R-5670 + R-60C, PP substrate, mesh fabric and PVC skin):
- 1Robotic spraying of substrate and skin
- 2Drying and activation in the oven
- 3Secondary infrared activation
- 4Mesh-fabric lamination
- 5Pressing and forming
We record dimensions, coat weight, temperature and cycle time on your line, then turn the validated parameters into work instructions.

Built for Hot, Humid and Cold Vehicles
| Test | Result | Condition |
|---|---|---|
| Humidity aging | 85% peel retention, no whitening or swelling | 60°C / 95% RH × 1,000 h |
| Low temperature | 92% peel retention | −40°C × 24 h |
| High temperature | 88% peel retention | 105°C × 24 h |
| Thermal cycling | No delamination; 85% retention | 100 cycles, −40°C ↔ 105°C |
| Chemical resistance | <6% strength loss | 72 h in neutral interior cleaner and silicone care fluid |
| Multi-substrate peel (180°) | ≥1,150 N/m microfiber / ABS; ≥980 N/m TPO / modified PP; ≥1,050 N/m PVC / wood-plastic board | 24 h after cure |
| BYD interior test (PHC honeycomb + flocked fabric) | 28.8 N → 30.7 N after 90°C × 168 h → 29.5 N after 10 humidity cycles; substrate failure in all | BYD interior standard; judged “pass” |
Humidity aging
- Result
- 85% peel retention, no whitening or swelling
- Condition
- 60°C / 95% RH × 1,000 h
Low temperature
- Result
- 92% peel retention
- Condition
- −40°C × 24 h
High temperature
- Result
- 88% peel retention
- Condition
- 105°C × 24 h
Thermal cycling
- Result
- No delamination; 85% retention
- Condition
- 100 cycles, −40°C ↔ 105°C
Chemical resistance
- Result
- <6% strength loss
- Condition
- 72 h in neutral interior cleaner and silicone care fluid
Multi-substrate peel (180°)
- Result
- ≥1,150 N/m microfiber / ABS; ≥980 N/m TPO / modified PP; ≥1,050 N/m PVC / wood-plastic board
- Condition
- 24 h after cure
BYD interior test (PHC honeycomb + flocked fabric)
- Result
- 28.8 N → 30.7 N after 90°C × 168 h → 29.5 N after 10 humidity cycles; substrate failure in all
- Condition
- BYD interior standard; judged “pass”
Typical lab values; test conditions stated. The BYD result is from RELANET test report RJTSC-26-7-2-001.
Where R-5670 Is Used
- Instrument panels
- High green strength on deep, curved surfaces
- Door panels and inserts
- Holds folded edges; proven on Nissan N7 programs and GAC Toyota Camry
- Armrests and center consoles
- Fast positioning on tight radii
- Seats
- Bonds fabric and leather to foam and plastic backs
- Trunk trim and spare wheel covers
- Flocked fabric on PP and PHC honeycomb; BYD Denza Z9GT
- Headliners
- Large-area spraying with consistent coat weight

In Series Production
| OEM | Program | Part |
|---|---|---|
| Dongfeng Nissan | N7 (LK1A), N6 (LK2A), NX7 (LK2C) | Interior wrapping |
| BYD / Denza | Z9GT | Spare wheel cover |
| BYD | Trunk trim (approved May 2026) | Trunk cover lamination |
| GAC Toyota | Camry | Door panel |
| GAC Toyota | Bozhi 3X | Interior trim |
Dongfeng Nissan
- Program
- N7 (LK1A), N6 (LK2A), NX7 (LK2C)
- Part
- Interior wrapping
BYD / Denza
- Program
- Z9GT
- Part
- Spare wheel cover
BYD
- Program
- Trunk trim (approved May 2026)
- Part
- Trunk cover lamination
GAC Toyota
- Program
- Camry
- Part
- Door panel
GAC Toyota
- Program
- Bozhi 3X
- Part
- Interior trim
One problem we solved: on the Nissan NX7 program, the line moved from solvent adhesive to waterborne. Early peel was only 5–10 N against a 19 N target. Our cross-testing showed the cause was the skin’s knit fabric, not the adhesive. Adding a nonwoven layer met the target.
Is 2K Waterborne PU Right for Your Part?
Water-based polyurethane adhesive fits most sprayed and wrapped interior parts. Here is when another technology fits better:
Choose waterborne PU when…
- You spray or wrap by hand, hot press or membrane press
- You need low VOC and a wide process window
- You are converting from solvent contact cement
Consider another technology when…
- You need a solvent-free, zero-drying roll-coating line → APAO or PUR hot melt
- The skin is backlit → light-transmitting adhesives
- You bond porous foam or felt → waterborne chloroprene
Frequently Asked Questions About RELANET R-5670
What mixing ratio should I use?
R-5670 : R-60C is 100 : 5–8 by weight. We set the exact ratio for your process during sampling; follow the current TDS.
Blue or clear curing agent?
Blue lets operators see coat weight and coverage, and most customers choose it. Use clear for light-colored or visible parts where no tint is allowed; it needs more careful spraying.
Does waterborne PU need surface treatment on PP?
Yes. Flame, corona or plasma treatment is normally needed on PP, and wrapping should follow within 4 hours. Our APAO R-7110 can bond qualified clean PP without pretreatment.
Doesn’t the extra drying step raise cost?
High solids mean less adhesive per m². A kilogram of waterborne adhesive carries roughly 500 g of solids, compared with about 100 g for solvent contact cement.
How should I store it in winter?
Keep it above 5°C in storage and transport. Below 4°C the dispersion freezes and cannot be recovered.
Can you adjust it for my line?
Yes. Open time, activation temperature, solids, tack balance and curing-agent color can be tuned. Custom samples take 7 working days.
Test R-5670 on Your Own Skin and Substrate
Send us 1–2 m² of your skin and substrate. We’ll run a free flat-panel test and send you the report, then support the first trial on your parts.
Need a custom version?Custom formulationPrefer email? anson@relanetadhesive.com